{"id":8430,"date":"2026-11-12T01:36:14","date_gmt":"2026-11-12T01:36:14","guid":{"rendered":"https:\/\/chinametalfoundry.com\/?p=8430"},"modified":"2026-11-13T04:05:29","modified_gmt":"2026-11-13T04:05:29","slug":"casting-melt-treatment","status":"publish","type":"post","link":"https:\/\/chinametalfoundry.com\/pl\/blog\/casting-melt-treatment\/","title":{"rendered":"Casting Melt Treatment: Degassing, Modification &#038; Melt Quality Control"},"content":{"rendered":"<article class=\"sc-article\" style=\"max-width: 820px; margin: 0 auto; font-family: 'Poppins',sans-serif; color: #7e7e7e; font-size: 16px; line-height: 1.7;\">\n<div class=\"sc-intro\" style=\"background: #F5F5F5; border-radius: 20px; padding: 22px 24px; font-style: italic; color: #3a3a3a; margin: 0 0 26px; line-height: 1.6;\">\n<p style=\"margin: 0;\"><strong style=\"color: #273171;\">Casting melt treatment<\/strong> is the short sequence of steps applied to metal between the furnace and the mold, and it decides whether the alloy on your drawing is the alloy you actually receive. Most buyers specify chemistry, tensile strength and X-ray class, then leave the molten-metal condition unwritten \u2014 which is exactly where hydrogen porosity, oxide films and unmodified eutectic silicon are decided.<\/p>\n<\/div>\n<p style=\"margin: 0 0 18px;\">This guide gives the numbers behind that window: hydrogen solubility ratios, density-index calculations, strontium and inoculant addition ranges, filtration selection, shop-floor release gates, and a worked payback model. Standards references are to <a style=\"color: #086ad4; text-decoration: none;\" href=\"https:\/\/store.astm.org\/standards\/e1251\" target=\"_blank\" rel=\"noopener\">ASTM E1251<\/a> for spark-AES chemistry, <a style=\"color: #086ad4; text-decoration: none;\" href=\"https:\/\/store.astm.org\/standards\/e155\" target=\"_blank\" rel=\"noopener\">ASTM E155<\/a> for reference radiographs, and the <a style=\"color: #086ad4; text-decoration: none;\" href=\"https:\/\/www.aluminum.org\/\" target=\"_blank\" rel=\"noopener\">Aluminum Association<\/a> for alloy and melt-handling practice. For the wider process context, start with our <a style=\"color: #086ad4; text-decoration: none;\" href=\"https:\/\/chinametalfoundry.com\/pl\/blog\/przewodnik-po-odlewaniu-metali\/\" target=\"_blank\" rel=\"noopener\">przewodnik po odlewaniu metali<\/a> and the <a style=\"color: #086ad4; text-decoration: none;\" href=\"https:\/\/chinametalfoundry.com\/pl\/blog\/metody-kontroli-odlewow\/\" target=\"_blank\" rel=\"noopener\">casting inspection methods overview<\/a>.<\/p>\n<figure style=\"margin: 24px 0;\"><img decoding=\"async\" style=\"width: 100%; display: block; border-radius: 4px;\" src=\"https:\/\/chinametalfoundry.com\/wp-content\/uploads\/2026\/11\/p262-casting-melt-treatment-1.webp\" alt=\"Casting melt treatment rotary degassing rotor immersed in a molten aluminum crucible\" \/><figcaption style=\"font-size: 13px; color: #7e7e7e; text-align: center; margin-top: 8px;\">Figure 1: rotary degassing in the transfer crucible \u2014 the last point where dissolved gas can still be removed.<\/figcaption><\/figure>\n<h2 style=\"font-family: 'Poppins',sans-serif; color: #273171; font-size: 25px; font-weight: 600; line-height: 1.3; margin: 34px 0 14px; padding: 4px 0 4px 30px; background: linear-gradient(to right, #ff512f 0px, #dd2476 5px, transparent 5px);\">What Casting Melt Treatment Actually Controls<\/h2>\n<p style=\"margin: 0 0 18px;\">A heat can meet its chemistry specification and still produce scrap. Casting melt treatment targets three variables that a spectrometer alone does not see, and each one is locked in the moment the metal enters the cavity. Once poured, no amount of <a style=\"color: #086ad4; text-decoration: none;\" href=\"https:\/\/chinametalfoundry.com\/pl\/blog\/obrobka-cieplna-odlewow\/\" target=\"_blank\" rel=\"noopener\">obr\u00f3bka cieplna<\/a> or machining restores them.<\/p>\n<ul style=\"margin: 0 0 18px; padding-left: 22px;\">\n<li style=\"margin: 0 0 8px;\"><strong style=\"color: #273171;\">Dissolved gas.<\/strong> Hydrogen in aluminum alloys, hydrogen and nitrogen in steels. Solubility collapses during solidification, so the excess precipitates as micro-porosity that reduces fatigue life and pressure tightness \u2014 the mechanism explained in our <a style=\"color: #086ad4; text-decoration: none;\" href=\"https:\/\/chinametalfoundry.com\/pl\/blog\/sand-casting-porosity-and-shrinkage\/\" target=\"_blank\" rel=\"noopener\">porosity and shrinkage analysis<\/a>.<\/li>\n<li style=\"margin: 0 0 8px;\"><strong style=\"color: #273171;\">Non-metallic inclusions.<\/strong> Oxide films, dross particles, refractory fragments and bifilms entrained by turbulence. These act as crack initiators and are more damaging to fatigue than equivalent-size gas pores.<\/li>\n<li style=\"margin: 0 0 8px;\"><strong style=\"color: #273171;\">Nucleation state.<\/strong> Eutectic silicon morphology in Al-Si alloys, graphite shape in irons, and as-cast grain size. Chemistry can be identical while elongation differs by a factor of two.<\/li>\n<\/ul>\n<p style=\"margin: 0 0 18px;\">The practical constraint is time. In aluminum sand and <a style=\"color: #086ad4; text-decoration: none;\" href=\"https:\/\/chinametalfoundry.com\/pl\/odlewanie-precyzyjne\/\" target=\"_blank\" rel=\"noopener\">odlewanie precyzyjne<\/a> the window from furnace tap to last pour is typically 8\u201315 minutes; for nodular iron it is 5\u201310 minutes before inoculation fades. That window is why casting melt treatment is a sequence with an order, not a list of optional additives: degas, then modify or inoculate, then filter, then pour and record.<\/p>\n<table style=\"width: 100%; border-collapse: collapse; margin: 18px 0 24px; font-size: 15px; color: #333333;\">\n<thead>\n<tr>\n<th style=\"background: #273171; color: #ffffff; padding: 12px 14px; text-align: left; font-weight: 600; border: 1px solid #273171;\">Variable<\/th>\n<th style=\"background: #273171; color: #ffffff; padding: 12px 14px; text-align: left; font-weight: 600; border: 1px solid #273171;\">Shop-floor measure<\/th>\n<th style=\"background: #273171; color: #ffffff; padding: 12px 14px; text-align: left; font-weight: 600; border: 1px solid #273171;\">Typical release criterion<\/th>\n<th style=\"background: #273171; color: #ffffff; padding: 12px 14px; text-align: left; font-weight: 600; border: 1px solid #273171;\">If it is missed<\/th>\n<\/tr>\n<\/thead>\n<tbody>\n<tr>\n<td style=\"border: 1px solid #E5E5E5; padding: 10px 14px;\">Dissolved hydrogen<\/td>\n<td style=\"border: 1px solid #E5E5E5; padding: 10px 14px;\">Reduced-pressure solidification sample, density index<\/td>\n<td style=\"border: 1px solid #E5E5E5; padding: 10px 14px;\">DI \u2264 2.0% for structural A356<\/td>\n<td style=\"border: 1px solid #E5E5E5; padding: 10px 14px;\">Micro-porosity, failed radiograph, leak test rejects<\/td>\n<\/tr>\n<tr style=\"background: #F5F5F5;\">\n<td style=\"border: 1px solid #E5E5E5; padding: 10px 14px;\">Oxide \/ dross<\/td>\n<td style=\"border: 1px solid #E5E5E5; padding: 10px 14px;\">Fracture sample, filter inspection, K-mold<\/td>\n<td style=\"border: 1px solid #E5E5E5; padding: 10px 14px;\">No continuous film on fracture face<\/td>\n<td style=\"border: 1px solid #E5E5E5; padding: 10px 14px;\">Fatigue failures, machined-surface tearing<\/td>\n<\/tr>\n<tr>\n<td style=\"border: 1px solid #E5E5E5; padding: 10px 14px;\">Modification level<\/td>\n<td style=\"border: 1px solid #E5E5E5; padding: 10px 14px;\">Thermal analysis cooling curve, eutectic undercooling \u0394TE<\/td>\n<td style=\"border: 1px solid #E5E5E5; padding: 10px 14px;\">\u0394TE 8\u201312 \u00b0C for Sr-modified A356<\/td>\n<td style=\"border: 1px solid #E5E5E5; padding: 10px 14px;\">Coarse plate-like silicon, elongation loss<\/td>\n<\/tr>\n<tr style=\"background: #F5F5F5;\">\n<td style=\"border: 1px solid #E5E5E5; padding: 10px 14px;\">Inoculation \/ nodularity<\/td>\n<td style=\"border: 1px solid #E5E5E5; padding: 10px 14px;\">Chill wedge, quick-cup microscopy<\/td>\n<td style=\"border: 1px solid #E5E5E5; padding: 10px 14px;\">Nodularity \u2265 85%, chill depth \u2264 3 mm<\/td>\n<td style=\"border: 1px solid #E5E5E5; padding: 10px 14px;\">Carbides, white iron edges, brittle castings<\/td>\n<\/tr>\n<tr>\n<td style=\"border: 1px solid #E5E5E5; padding: 10px 14px;\">Chemistry<\/td>\n<td style=\"border: 1px solid #E5E5E5; padding: 10px 14px;\">Spark-AES per <a style=\"color: #086ad4; text-decoration: none;\" href=\"https:\/\/store.astm.org\/standards\/e1251\" target=\"_blank\" rel=\"noopener\">ASTM E1251<\/a><\/td>\n<td style=\"border: 1px solid #E5E5E5; padding: 10px 14px;\">Within alloy limits before tap<\/td>\n<td style=\"border: 1px solid #E5E5E5; padding: 10px 14px;\">Off-grade heat, wrong T6 response<\/td>\n<\/tr>\n<\/tbody>\n<\/table>\n<p style=\"margin: 0 0 18px;\">Note the last row. Casting melt treatment records are the only place these three variables appear together; chemistry is a gate, not a result: a heat inside specification can still carry 0.25 mL\/100 g of hydrogen. Buyers who audit only the certificate are auditing the easiest 20% of the problem \u2014 a pattern that shows up repeatedly in <a style=\"color: #086ad4; text-decoration: none;\" href=\"https:\/\/chinametalfoundry.com\/pl\/blog\/casting-scrap-rate\/\" target=\"_blank\" rel=\"noopener\">scrap-rate investigations<\/a>.<\/p>\n<h2 style=\"font-family: 'Poppins',sans-serif; color: #273171; font-size: 25px; font-weight: 600; line-height: 1.3; margin: 34px 0 14px; padding: 4px 0 4px 30px; background: linear-gradient(to right, #ff512f 0px, #dd2476 5px, transparent 5px);\">Degassing: Hydrogen, Density Index and the Reduced-Pressure Test<\/h2>\n<p style=\"margin: 0 0 18px;\">Hydrogen solubility in liquid aluminum near 700\u2013750 \u00b0C is roughly 0.6\u20130.9 mL per 100 g, while the solid metal holds only about 0.03\u20130.05 mL per 100 g. That 15\u201320\u00d7 drop is the whole reason gas porosity exists: the excess has to go somewhere, and it goes into interdendritic voids. Casting melt treatment removes it before the metal sees a mold.<\/p>\n<p style=\"margin: 0 0 18px;\">In casting melt treatment, rotary degassing uses a graphite impeller at 300\u2013550 rpm with argon or nitrogen at 6\u201315 L\/min for 6\u201312 minutes per batch. Fine, inert bubbles sweep dissolved hydrogen out and float oxides to the dross layer. A one-tonne crucible commonly needs 8\u201310 minutes to reach a density index below 2%; doubling the gas flow does not halve that time, because the limit is bubble\u2013metal contact area, not gas volume.<\/p>\n<p style=\"margin: 0 0 18px;\">The reduced-pressure test solidifies a small sample under roughly 80\u2013100 mbar alongside a sample solidified at atmospheric pressure. The density index is then: <strong style=\"color: #273171;\">DI = (D_atm \u2212 D_vac) \/ D_atm \u00d7 100%<\/strong>. A worked example: D_atm = 2.682 g\/cm\u00b3 and D_vac = 2.641 g\/cm\u00b3 gives (0.041 \/ 2.682) \u00d7 100 = <strong style=\"color: #273171;\">1.53%<\/strong>, an acceptable structural melt. Drop D_vac to 2.605 and the same arithmetic gives 2.87%, which should be re-degassed rather than poured.<\/p>\n<table style=\"width: 100%; border-collapse: collapse; margin: 18px 0 24px; font-size: 15px; color: #333333;\">\n<thead>\n<tr>\n<th style=\"background: #273171; color: #ffffff; padding: 12px 14px; text-align: left; font-weight: 600; border: 1px solid #273171;\">Density index<\/th>\n<th style=\"background: #273171; color: #ffffff; padding: 12px 14px; text-align: left; font-weight: 600; border: 1px solid #273171;\">Approx. hydrogen level<\/th>\n<th style=\"background: #273171; color: #ffffff; padding: 12px 14px; text-align: left; font-weight: 600; border: 1px solid #273171;\">Typical application<\/th>\n<th style=\"background: #273171; color: #ffffff; padding: 12px 14px; text-align: left; font-weight: 600; border: 1px solid #273171;\">Action<\/th>\n<\/tr>\n<\/thead>\n<tbody>\n<tr>\n<td style=\"border: 1px solid #E5E5E5; padding: 10px 14px;\">&lt; 1.0%<\/td>\n<td style=\"border: 1px solid #E5E5E5; padding: 10px 14px;\">Low, &lt; 0.10 mL\/100 g<\/td>\n<td style=\"border: 1px solid #E5E5E5; padding: 10px 14px;\">Pressure-tight housings, aerospace-class radiography<\/td>\n<td style=\"border: 1px solid #E5E5E5; padding: 10px 14px;\">Pour within 10 min<\/td>\n<\/tr>\n<tr style=\"background: #F5F5F5;\">\n<td style=\"border: 1px solid #E5E5E5; padding: 10px 14px;\">1.0\u20132.0%<\/td>\n<td style=\"border: 1px solid #E5E5E5; padding: 10px 14px;\">0.10\u20130.15 mL\/100 g<\/td>\n<td style=\"border: 1px solid #E5E5E5; padding: 10px 14px;\">Structural A356-T6, hydraulic bodies<\/td>\n<td style=\"border: 1px solid #E5E5E5; padding: 10px 14px;\">Normal release<\/td>\n<\/tr>\n<tr>\n<td style=\"border: 1px solid #E5E5E5; padding: 10px 14px;\">2.0\u20134.0%<\/td>\n<td style=\"border: 1px solid #E5E5E5; padding: 10px 14px;\">0.15\u20130.25 mL\/100 g<\/td>\n<td style=\"border: 1px solid #E5E5E5; padding: 10px 14px;\">Non-critical brackets, cosmetic parts<\/td>\n<td style=\"border: 1px solid #E5E5E5; padding: 10px 14px;\">Re-degas if X-ray class is specified<\/td>\n<\/tr>\n<tr style=\"background: #F5F5F5;\">\n<td style=\"border: 1px solid #E5E5E5; padding: 10px 14px;\">&gt; 4.0%<\/td>\n<td style=\"border: 1px solid #E5E5E5; padding: 10px 14px;\">&gt; 0.25 mL\/100 g<\/td>\n<td style=\"border: 1px solid #E5E5E5; padding: 10px 14px;\">None for quality castings<\/td>\n<td style=\"border: 1px solid #E5E5E5; padding: 10px 14px;\">Hold the heat, find the moisture source<\/td>\n<\/tr>\n<\/tbody>\n<\/table>\n<h3 style=\"font-family: 'Poppins',sans-serif; color: #273171; font-size: 20px; font-weight: 600; line-height: 1.4; margin: 26px 0 8px; text-transform: capitalize;\">Why a clean-looking surface still fails X-ray<\/h3>\n<hr style=\"width: 100px; height: 4px; background: #EF890D; border: none; border-radius: 2px; margin: 0 0 14px; line-height: 0; opacity: 1;\" \/>\n<p style=\"margin: 0 0 18px;\">Gas pores are internal and invisible on a ground surface, so visual inspection is not a release test. Reference radiographs such as <a style=\"color: #086ad4; text-decoration: none;\" href=\"https:\/\/store.astm.org\/standards\/e155\" target=\"_blank\" rel=\"noopener\">ASTM E155<\/a> classify severity, but they only describe the result \u2014 they cannot tell you whether the cause was hydrogen, shrinkage or an oxide film. That distinction is why <a style=\"color: #086ad4; text-decoration: none;\" href=\"https:\/\/chinametalfoundry.com\/pl\/blog\/casting-simulation\/\" target=\"_blank\" rel=\"noopener\">solidification simulation<\/a> and a melt record have to be read together: a pore cluster in a hot spot is feeding, while uniformly distributed fine porosity across every section is gas.<\/p>\n<p style=\"margin: 0 0 18px;\">Re-gassing is the underrated failure mode. A degassed bath held in humid air can climb from 1.5% to above 3% DI within 20\u201330 minutes, because moisture in the atmosphere and on damp tools reacts at the metal surface. The discipline that makes casting melt treatment work is therefore procedural: dry ladles, covered crucibles, and a hard rule that metal not poured within 10 minutes of the DI reading is re-tested. High-volume <a style=\"color: #086ad4; text-decoration: none;\" href=\"https:\/\/chinametalfoundry.com\/pl\/uslugi-odlewania-cisnieniowego\/\" target=\"_blank\" rel=\"noopener\">odlewanie ci\u015bnieniowe<\/a> cells automate this with inline degassing; jobbing <a style=\"color: #086ad4; text-decoration: none;\" href=\"https:\/\/chinametalfoundry.com\/pl\/odlewanie-w-formach-piaskowych\/\" target=\"_blank\" rel=\"noopener\">odlewanie w formach piaskowych<\/a> shops need the written rule instead.<\/p>\n<figure style=\"margin: 24px 0;\"><img decoding=\"async\" style=\"width: 100%; display: block; border-radius: 4px;\" src=\"https:\/\/chinametalfoundry.com\/wp-content\/uploads\/2026\/11\/p262-casting-melt-treatment-2.webp\" alt=\"Casting melt treatment reduced pressure solidified samples with ceramic foam filter and spectrometer disc\" \/><figcaption style=\"font-size: 13px; color: #7e7e7e; text-align: center; margin-top: 8px;\">Figure 2: reduced-pressure samples, a spectrometer disc and a ceramic foam filter \u2014 the three physical records of a released heat.<\/figcaption><\/figure>\n<h2 style=\"font-family: 'Poppins',sans-serif; color: #273171; font-size: 25px; font-weight: 600; line-height: 1.3; margin: 34px 0 14px; padding: 4px 0 4px 30px; background: linear-gradient(to right, #ff512f 0px, #dd2476 5px, transparent 5px);\">Modification and Grain Refinement in Aluminum Castings<\/h2>\n<p style=\"margin: 0 0 18px;\">Unmodified A356 contains coarse, plate-like eutectic silicon. In the T6 condition that microstructure typically delivers 3\u20135% elongation; with proper strontium modification the silicon becomes fibrous and the same alloy reaches 8\u201312%. Casting melt treatment changes ductility without changing the chemistry certificate, which is why a buyer who specifies only the alloy designation has not actually specified the property they need.<\/p>\n<p style=\"margin: 0 0 18px;\">Strontium is added as an Al-Sr10 master alloy at 100\u2013200 ppm target residual, with real-world recovery of 60\u201380%. It needs 15\u201330 minutes of dissolution and gentle stirring to homogenize, and it fades over 3\u20134 hours of holding. Push past roughly 300 ppm and the treatment becomes counterproductive: over-modification coarsens the eutectic again and increases micro-porosity, especially when hydrogen is not under control first. Sodium at 0.008\u20130.02% works faster but fades in 30\u201360 minutes and contaminates crucibles, so it has largely been displaced in production foundries.<\/p>\n<p style=\"margin: 0 0 18px;\">Grain refinement is a separate objective, and both additions live inside casting melt treatment rather than the alloy specification. An Al-5Ti-1B addition targeting 0.10\u20130.15% Ti and about 0.02% B can reduce as-cast grain size from 400\u2013800 \u00b5m to 100\u2013200 \u00b5m, cutting hot tearing in constrained geometries and improving feeding in thin sections. It is not a substitute for modification: one controls grain size, the other controls eutectic morphology. Alloy choice still sets the ceiling \u2014 see the <a style=\"color: #086ad4; text-decoration: none;\" href=\"https:\/\/chinametalfoundry.com\/pl\/blog\/aluminum-casting-alloys-a356-vs-a380\/\" target=\"_blank\" rel=\"noopener\">A356 versus A380 comparison<\/a> oraz nasz <a style=\"color: #086ad4; text-decoration: none;\" href=\"https:\/\/chinametalfoundry.com\/pl\/blog\/casting-material-substitution\/\" target=\"_blank\" rel=\"noopener\">material substitution analysis<\/a>.<\/p>\n<table style=\"width: 100%; border-collapse: collapse; margin: 18px 0 24px; font-size: 15px; color: #333333;\">\n<thead>\n<tr>\n<th style=\"background: #273171; color: #ffffff; padding: 12px 14px; text-align: left; font-weight: 600; border: 1px solid #273171;\">Addition<\/th>\n<th style=\"background: #273171; color: #ffffff; padding: 12px 14px; text-align: left; font-weight: 600; border: 1px solid #273171;\">Typical target<\/th>\n<th style=\"background: #273171; color: #ffffff; padding: 12px 14px; text-align: left; font-weight: 600; border: 1px solid #273171;\">Effective window<\/th>\n<th style=\"background: #273171; color: #ffffff; padding: 12px 14px; text-align: left; font-weight: 600; border: 1px solid #273171;\">Verification<\/th>\n<th style=\"background: #273171; color: #ffffff; padding: 12px 14px; text-align: left; font-weight: 600; border: 1px solid #273171;\">Main risk<\/th>\n<\/tr>\n<\/thead>\n<tbody>\n<tr>\n<td style=\"border: 1px solid #E5E5E5; padding: 10px 14px;\">Al-Sr10 (modification)<\/td>\n<td style=\"border: 1px solid #E5E5E5; padding: 10px 14px;\">100\u2013200 ppm Sr residual<\/td>\n<td style=\"border: 1px solid #E5E5E5; padding: 10px 14px;\">3\u20134 h holding<\/td>\n<td style=\"border: 1px solid #E5E5E5; padding: 10px 14px;\">Thermal analysis \u0394TE 8\u201312 \u00b0C<\/td>\n<td style=\"border: 1px solid #E5E5E5; padding: 10px 14px;\">Over-modification &gt; 300 ppm raises porosity<\/td>\n<\/tr>\n<tr style=\"background: #F5F5F5;\">\n<td style=\"border: 1px solid #E5E5E5; padding: 10px 14px;\">Na-based modifier<\/td>\n<td style=\"border: 1px solid #E5E5E5; padding: 10px 14px;\">0.008\u20130.02% Na<\/td>\n<td style=\"border: 1px solid #E5E5E5; padding: 10px 14px;\">30\u201360 min<\/td>\n<td style=\"border: 1px solid #E5E5E5; padding: 10px 14px;\">Fracture \/ thermal analysis<\/td>\n<td style=\"border: 1px solid #E5E5E5; padding: 10px 14px;\">Fast fade, tool contamination<\/td>\n<\/tr>\n<tr>\n<td style=\"border: 1px solid #E5E5E5; padding: 10px 14px;\">Al-5Ti-1B (refiner)<\/td>\n<td style=\"border: 1px solid #E5E5E5; padding: 10px 14px;\">0.10\u20130.15% Ti, ~0.02% B<\/td>\n<td style=\"border: 1px solid #E5E5E5; padding: 10px 14px;\">2\u20134 h<\/td>\n<td style=\"border: 1px solid #E5E5E5; padding: 10px 14px;\">Grain size on quick-cup sample<\/td>\n<td style=\"border: 1px solid #E5E5E5; padding: 10px 14px;\">Settling of TiB\u2082 particles in long holds<\/td>\n<\/tr>\n<tr style=\"background: #F5F5F5;\">\n<td style=\"border: 1px solid #E5E5E5; padding: 10px 14px;\">Rotary degassing<\/td>\n<td style=\"border: 1px solid #E5E5E5; padding: 10px 14px;\">DI \u2264 2.0%<\/td>\n<td style=\"border: 1px solid #E5E5E5; padding: 10px 14px;\">Re-test after 10 min<\/td>\n<td style=\"border: 1px solid #E5E5E5; padding: 10px 14px;\">Reduced-pressure density index<\/td>\n<td style=\"border: 1px solid #E5E5E5; padding: 10px 14px;\">Re-gassing from humid air<\/td>\n<\/tr>\n<tr>\n<td style=\"border: 1px solid #E5E5E5; padding: 10px 14px;\">Ceramic foam filter<\/td>\n<td style=\"border: 1px solid #E5E5E5; padding: 10px 14px;\">10\u201330 ppi, 15\u201325 mm<\/td>\n<td style=\"border: 1px solid #E5E5E5; padding: 10px 14px;\">Single pour<\/td>\n<td style=\"border: 1px solid #E5E5E5; padding: 10px 14px;\">Visual + \u0394P across filter<\/td>\n<td style=\"border: 1px solid #E5E5E5; padding: 10px 14px;\">Blockage if metal is cold<\/td>\n<\/tr>\n<\/tbody>\n<\/table>\n<h3 style=\"font-family: 'Poppins',sans-serif; color: #273171; font-size: 20px; font-weight: 600; line-height: 1.4; margin: 26px 0 8px; text-transform: capitalize;\">Read the cooling curve, not just the chemistry<\/h3>\n<hr style=\"width: 100px; height: 4px; background: #EF890D; border: none; border-radius: 2px; margin: 0 0 14px; line-height: 0; opacity: 1;\" \/>\n<p style=\"margin: 0 0 18px;\">Thermal analysis is the cheapest inline verification of modification level. A small quick-cup sample produces a cooling curve whose eutectic arrest shifts: unmodified A356 shows almost no eutectic undercooling, while a well-modified melt shows \u0394TE of 8\u201312 \u00b0C. Foundries that log \u0394TE per ladle can catch a missed Sr addition before 200 kg of metal is poured, rather than discovering low elongation after <a style=\"color: #086ad4; text-decoration: none;\" href=\"https:\/\/chinametalfoundry.com\/pl\/blog\/obrobka-cieplna-odlewow\/\" target=\"_blank\" rel=\"noopener\">T6 heat treatment<\/a> oraz <a style=\"color: #086ad4; text-decoration: none;\" href=\"https:\/\/chinametalfoundry.com\/pl\/cnc-machining-services\/\" target=\"_blank\" rel=\"noopener\">Obr\u00f3bka CNC<\/a> have already added value to the batch.<\/p>\n<p style=\"margin: 0 0 18px;\">This is also where a casting melt treatment record protects both sides commercially. If a buyer later files a <a style=\"color: #086ad4; text-decoration: none;\" href=\"https:\/\/chinametalfoundry.com\/pl\/blog\/casting-defect-claim\/\" target=\"_blank\" rel=\"noopener\">defect claim<\/a>, the \u0394TE and DI logs tied to a heat number show whether the loss came from the melt or from downstream handling \u2014 a distinction that our <a style=\"color: #086ad4; text-decoration: none;\" href=\"https:\/\/chinametalfoundry.com\/pl\/blog\/umowa-dotyczaca-jakosci-odlewow\/\" target=\"_blank\" rel=\"noopener\">quality agreement template<\/a> treats as a defined evidence item.<\/p>\n<h2 style=\"font-family: 'Poppins',sans-serif; color: #273171; font-size: 25px; font-weight: 600; line-height: 1.3; margin: 34px 0 14px; padding: 4px 0 4px 30px; background: linear-gradient(to right, #ff512f 0px, #dd2476 5px, transparent 5px);\">Inoculation and Nodularizing for Iron Castings<\/h2>\n<p style=\"margin: 0 0 18px;\">In iron, casting melt treatment is about graphite. Nodularizing with magnesium converts graphite from flakes to spheroids; inoculation then provides the nuclei that decide how many spheroids form and whether carbides appear in thin edges. Both steps decay with time, so the clock starts the moment the treatment ladle is filled.<\/p>\n<p style=\"margin: 0 0 18px;\">For ductile iron, base sulfur should be below about 0.02% before Mg treatment, with residual Mg held at 0.03\u20130.06%. Below 0.03% the graphite reverts to compacted or flake forms; above 0.06% the melt is prone to dross, carbide formation and shrinkage. A well-treated ASTM A536 65-45-12 heat targets nodularity \u2265 85% and a nodule count above roughly 100\/mm\u00b2 in a 25 mm section. The difference is mechanical: gray iron with type-A graphite runs 200\u2013300 MPa tensile with near-zero elongation, while 65-45-12 reaches about 450 MPa with 12% elongation \u2014 see the <a style=\"color: #086ad4; text-decoration: none;\" href=\"https:\/\/chinametalfoundry.com\/pl\/blog\/zeliwo-szare-a-zeliwo-sferoidalne\/\" target=\"_blank\" rel=\"noopener\">gray iron versus ductile iron comparison<\/a>.<\/p>\n<table style=\"width: 100%; border-collapse: collapse; margin: 18px 0 24px; font-size: 15px; color: #333333;\">\n<thead>\n<tr>\n<th style=\"background: #273171; color: #ffffff; padding: 12px 14px; text-align: left; font-weight: 600; border: 1px solid #273171;\">Practice<\/th>\n<th style=\"background: #273171; color: #ffffff; padding: 12px 14px; text-align: left; font-weight: 600; border: 1px solid #273171;\">Addition rate<\/th>\n<th style=\"background: #273171; color: #ffffff; padding: 12px 14px; text-align: left; font-weight: 600; border: 1px solid #273171;\">Effective window<\/th>\n<th style=\"background: #273171; color: #ffffff; padding: 12px 14px; text-align: left; font-weight: 600; border: 1px solid #273171;\">Chill \/ carbide risk<\/th>\n<th style=\"background: #273171; color: #ffffff; padding: 12px 14px; text-align: left; font-weight: 600; border: 1px solid #273171;\">Where it fits<\/th>\n<\/tr>\n<\/thead>\n<tbody>\n<tr>\n<td style=\"border: 1px solid #E5E5E5; padding: 10px 14px;\">Ladle inoculation (FeSi75)<\/td>\n<td style=\"border: 1px solid #E5E5E5; padding: 10px 14px;\">0.2\u20130.6%<\/td>\n<td style=\"border: 1px solid #E5E5E5; padding: 10px 14px;\">5\u201312 min<\/td>\n<td style=\"border: 1px solid #E5E5E5; padding: 10px 14px;\">Rises steeply after 8 min<\/td>\n<td style=\"border: 1px solid #E5E5E5; padding: 10px 14px;\">General sand castings<\/td>\n<\/tr>\n<tr style=\"background: #F5F5F5;\">\n<td style=\"border: 1px solid #E5E5E5; padding: 10px 14px;\">Stream inoculation<\/td>\n<td style=\"border: 1px solid #E5E5E5; padding: 10px 14px;\">0.05\u20130.15%<\/td>\n<td style=\"border: 1px solid #E5E5E5; padding: 10px 14px;\">At pour only<\/td>\n<td style=\"border: 1px solid #E5E5E5; padding: 10px 14px;\">Low<\/td>\n<td style=\"border: 1px solid #E5E5E5; padding: 10px 14px;\">Thin-section, high-nodularity parts<\/td>\n<\/tr>\n<tr>\n<td style=\"border: 1px solid #E5E5E5; padding: 10px 14px;\">In-mold inoculation<\/td>\n<td style=\"border: 1px solid #E5E5E5; padding: 10px 14px;\">0.05\u20130.10%<\/td>\n<td style=\"border: 1px solid #E5E5E5; padding: 10px 14px;\">At pour only<\/td>\n<td style=\"border: 1px solid #E5E5E5; padding: 10px 14px;\">Lowest<\/td>\n<td style=\"border: 1px solid #E5E5E5; padding: 10px 14px;\">Automated high-volume lines<\/td>\n<\/tr>\n<tr style=\"background: #F5F5F5;\">\n<td style=\"border: 1px solid #E5E5E5; padding: 10px 14px;\">Mg treatment (FeSiMg)<\/td>\n<td style=\"border: 1px solid #E5E5E5; padding: 10px 14px;\">Residual Mg 0.03\u20130.06%<\/td>\n<td style=\"border: 1px solid #E5E5E5; padding: 10px 14px;\">8\u201312 min before fade<\/td>\n<td style=\"border: 1px solid #E5E5E5; padding: 10px 14px;\">Excess Mg promotes carbides<\/td>\n<td style=\"border: 1px solid #E5E5E5; padding: 10px 14px;\">All nodular irons<\/td>\n<\/tr>\n<tr>\n<td style=\"border: 1px solid #E5E5E5; padding: 10px 14px;\">No treatment<\/td>\n<td style=\"border: 1px solid #E5E5E5; padding: 10px 14px;\">\u2014<\/td>\n<td style=\"border: 1px solid #E5E5E5; padding: 10px 14px;\">\u2014<\/td>\n<td style=\"border: 1px solid #E5E5E5; padding: 10px 14px;\">White iron in thin edges<\/td>\n<td style=\"border: 1px solid #E5E5E5; padding: 10px 14px;\">Only for non-structural counterweights<\/td>\n<\/tr>\n<\/tbody>\n<\/table>\n<h3 style=\"font-family: 'Poppins',sans-serif; color: #273171; font-size: 20px; font-weight: 600; line-height: 1.4; margin: 26px 0 8px; text-transform: capitalize;\">The eight-minute rule on the shop floor<\/h3>\n<hr style=\"width: 100px; height: 4px; background: #EF890D; border: none; border-radius: 2px; margin: 0 0 14px; line-height: 0; opacity: 1;\" \/>\n<p style=\"margin: 0 0 18px;\">Inoculation fade is not gradual in a way that operators can eyeball. A chill wedge poured immediately after inoculation might show 2 mm of white iron; the same metal poured eight minutes later can show 6 mm and produce hard spots that destroy tool life in <a style=\"color: #086ad4; text-decoration: none;\" href=\"https:\/\/chinametalfoundry.com\/pl\/cnc-machining-services\/\" target=\"_blank\" rel=\"noopener\">machining<\/a>. The operational answer is late inoculation \u2014 stream or in-mold \u2014 plus a hard maximum ladle-to-pour interval written into the work instruction. For alloy and grade selection beyond ductile iron, see <a style=\"color: #086ad4; text-decoration: none;\" href=\"https:\/\/chinametalfoundry.com\/pl\/blog\/cast-steel-grades\/\" target=\"_blank\" rel=\"noopener\">cast steel grades<\/a> oraz <a style=\"color: #086ad4; text-decoration: none;\" href=\"https:\/\/chinametalfoundry.com\/pl\/blog\/high-chrome-white-iron-castings\/\" target=\"_blank\" rel=\"noopener\">high-chrome white iron<\/a>.<\/p>\n<p style=\"margin: 0 0 18px;\">Iron work also ties directly to the mold: a well-inoculated melt will still shrink if the riser and gating are wrong. Treat the <a style=\"color: #086ad4; text-decoration: none;\" href=\"https:\/\/chinametalfoundry.com\/pl\/blog\/projektowanie-kanalow-wlewowych\/\" target=\"_blank\" rel=\"noopener\">riser design guidance<\/a> oraz <a style=\"color: #086ad4; text-decoration: none;\" href=\"https:\/\/chinametalfoundry.com\/pl\/blog\/wzory-do-projektowania-form-odlewniczych\/\" target=\"_blank\" rel=\"noopener\">pattern and mold design notes<\/a> as parallel inputs, and use <a style=\"color: #086ad4; text-decoration: none;\" href=\"https:\/\/chinametalfoundry.com\/pl\/rozwiazania\/odlewy-zeliwne\/\" target=\"_blank\" rel=\"noopener\">iron casting solutions<\/a> when specifying the production route rather than a single heat.<\/p>\n<figure style=\"margin: 24px 0;\"><img decoding=\"async\" style=\"width: 100%; display: block; border-radius: 4px;\" src=\"https:\/\/chinametalfoundry.com\/wp-content\/uploads\/2026\/11\/p262-casting-melt-treatment-3.webp\" alt=\"Casting melt treatment inoculation wire coil ferrosilicon lumps and transfer ladle on foundry bench\" \/><figcaption style=\"font-size: 13px; color: #7e7e7e; text-align: center; margin-top: 8px;\">Figure 3: inoculant wire, ferrosilicon lumps and a transfer ladle \u2014 the consumables whose timing determines graphite shape.<\/figcaption><\/figure>\n<h2 style=\"font-family: 'Poppins',sans-serif; color: #273171; font-size: 25px; font-weight: 600; line-height: 1.3; margin: 34px 0 14px; padding: 4px 0 4px 30px; background: linear-gradient(to right, #ff512f 0px, #dd2476 5px, transparent 5px);\">Inclusion Control: Filtration and Charge Cleanliness<\/h2>\n<p style=\"margin: 0 0 18px;\">Degassing removes gas; it does not remove oxide films already in the metal. Bifilms \u2014 folded surface oxide entrained during pouring or transfer \u2014 behave like pre-existing cracks, and they are the usual explanation when two heats with identical DI values produce very different fatigue results. Casting melt treatment handles inclusions through charge discipline, quiet transfer and filtration.<\/p>\n<p style=\"margin: 0 0 18px;\">Ceramic foam filters at 10\u201330 ppi and 15\u201325 mm thickness are placed in the runner or pouring cup. They work by impingement and adhesion rather than simple sieving, so metal velocity matters more than nominal pore size: keep flow near 0.5\u20131.0 kg\/s per 100 \u00d7 100 mm of filter area. Under those conditions, capture of inclusions above roughly 20 \u00b5m is commonly 70\u201390%. A filter that is too fine for the pour rate simply raises the head requirement and can freeze off the runner.<\/p>\n<table style=\"width: 100%; border-collapse: collapse; margin: 18px 0 24px; font-size: 15px; color: #333333;\">\n<thead>\n<tr>\n<th style=\"background: #273171; color: #ffffff; padding: 12px 14px; text-align: left; font-weight: 600; border: 1px solid #273171;\">Filter<\/th>\n<th style=\"background: #273171; color: #ffffff; padding: 12px 14px; text-align: left; font-weight: 600; border: 1px solid #273171;\">Typical alloy \/ process<\/th>\n<th style=\"background: #273171; color: #ffffff; padding: 12px 14px; text-align: left; font-weight: 600; border: 1px solid #273171;\">Part type<\/th>\n<th style=\"background: #273171; color: #ffffff; padding: 12px 14px; text-align: left; font-weight: 600; border: 1px solid #273171;\">Relative pressure drop<\/th>\n<th style=\"background: #273171; color: #ffffff; padding: 12px 14px; text-align: left; font-weight: 600; border: 1px solid #273171;\">Notes<\/th>\n<\/tr>\n<\/thead>\n<tbody>\n<tr>\n<td style=\"border: 1px solid #E5E5E5; padding: 10px 14px;\">10 ppi, 20 mm<\/td>\n<td style=\"border: 1px solid #E5E5E5; padding: 10px 14px;\">Iron and steel, sand casting<\/td>\n<td style=\"border: 1px solid #E5E5E5; padding: 10px 14px;\">Heavy sections, high flow<\/td>\n<td style=\"border: 1px solid #E5E5E5; padding: 10px 14px;\">Low<\/td>\n<td style=\"border: 1px solid #E5E5E5; padding: 10px 14px;\">Coarse dross capture; pair with a dross trap<\/td>\n<\/tr>\n<tr style=\"background: #F5F5F5;\">\n<td style=\"border: 1px solid #E5E5E5; padding: 10px 14px;\">20 ppi, 20 mm<\/td>\n<td style=\"border: 1px solid #E5E5E5; padding: 10px 14px;\">Aluminum sand and gravity die<\/td>\n<td style=\"border: 1px solid #E5E5E5; padding: 10px 14px;\">Housings, manifolds<\/td>\n<td style=\"border: 1px solid #E5E5E5; padding: 10px 14px;\">Medium<\/td>\n<td style=\"border: 1px solid #E5E5E5; padding: 10px 14px;\">Most common general-purpose choice<\/td>\n<\/tr>\n<tr>\n<td style=\"border: 1px solid #E5E5E5; padding: 10px 14px;\">30 ppi, 15 mm<\/td>\n<td style=\"border: 1px solid #E5E5E5; padding: 10px 14px;\">Aluminum investment, thin walls<\/td>\n<td style=\"border: 1px solid #E5E5E5; padding: 10px 14px;\">Precision, pressure-tight parts<\/td>\n<td style=\"border: 1px solid #E5E5E5; padding: 10px 14px;\">Wysoki<\/td>\n<td style=\"border: 1px solid #E5E5E5; padding: 10px 14px;\">Needs adequate metallostatic head<\/td>\n<\/tr>\n<tr style=\"background: #F5F5F5;\">\n<td style=\"border: 1px solid #E5E5E5; padding: 10px 14px;\">No filter<\/td>\n<td style=\"border: 1px solid #E5E5E5; padding: 10px 14px;\">Non-critical counterweights<\/td>\n<td style=\"border: 1px solid #E5E5E5; padding: 10px 14px;\">Cosmetic \/ balance weights<\/td>\n<td style=\"border: 1px solid #E5E5E5; padding: 10px 14px;\">None<\/td>\n<td style=\"border: 1px solid #E5E5E5; padding: 10px 14px;\">Only where radiographic class is unspecified<\/td>\n<\/tr>\n<\/tbody>\n<\/table>\n<p style=\"margin: 0 0 18px;\">Charge cleanliness is the cheaper half of casting melt treatment. Cap returns at 30\u201340% of the charge, degrease and dry them before charging, and avoid plunging damp tools into the bath. The <a style=\"color: #086ad4; text-decoration: none;\" href=\"https:\/\/www.aluminum.org\/\" target=\"_blank\" rel=\"noopener\">Aluminum Association<\/a> publishes melt-handling and alloy practice that is a reasonable baseline for supplier audits. Where a supplier cannot produce filter and charge records, treat the <a style=\"color: #086ad4; text-decoration: none;\" href=\"https:\/\/chinametalfoundry.com\/pl\/blog\/casting-incoming-inspection-plan\/\" target=\"_blank\" rel=\"noopener\">incoming inspection plan<\/a> as the fallback control rather than assuming the melt was clean.<\/p>\n<p style=\"margin: 0 0 18px;\">Downstream, the distinction matters commercially. Weld repair can close a surface defect but cannot remove distributed oxide films \u2014 our <a style=\"color: #086ad4; text-decoration: none;\" href=\"https:\/\/chinametalfoundry.com\/pl\/blog\/casting-weld-repair\/\" target=\"_blank\" rel=\"noopener\">weld repair guide<\/a> oraz <a style=\"color: #086ad4; text-decoration: none;\" href=\"https:\/\/chinametalfoundry.com\/pl\/blog\/casting-nonconformance\/\" target=\"_blank\" rel=\"noopener\">nonconformance disposition framework<\/a> both draw that line. Specifying casting melt treatment upstream is cheaper than arguing about disposition after the parts have been machined.<\/p>\n<h2 style=\"font-family: 'Poppins',sans-serif; color: #273171; font-size: 25px; font-weight: 600; line-height: 1.3; margin: 34px 0 14px; padding: 4px 0 4px 30px; background: linear-gradient(to right, #ff512f 0px, #dd2476 5px, transparent 5px);\">Measuring Casting Melt Treatment Before You Pour<\/h2>\n<p style=\"margin: 0 0 18px;\">A treatment that is not measured is a claim, not a control. The minimum credible shop-floor package has four instruments: a spark-AES spectrometer for chemistry (sampled per <a style=\"color: #086ad4; text-decoration: none;\" href=\"https:\/\/store.astm.org\/standards\/e1251\" target=\"_blank\" rel=\"noopener\">ASTM E1251<\/a>), a thermal-analysis quick-cup for modification or inoculation level, a reduced-pressure solidification unit for density index, and a documented filter \/ dross check. None of them is expensive relative to a scrapped batch.<\/p>\n<table style=\"width: 100%; border-collapse: collapse; margin: 18px 0 24px; font-size: 15px; color: #333333;\">\n<thead>\n<tr>\n<th style=\"background: #273171; color: #ffffff; padding: 12px 14px; text-align: left; font-weight: 600; border: 1px solid #273171;\">Check<\/th>\n<th style=\"background: #273171; color: #ffffff; padding: 12px 14px; text-align: left; font-weight: 600; border: 1px solid #273171;\">Method<\/th>\n<th style=\"background: #273171; color: #ffffff; padding: 12px 14px; text-align: left; font-weight: 600; border: 1px solid #273171;\">Frequency<\/th>\n<th style=\"background: #273171; color: #ffffff; padding: 12px 14px; text-align: left; font-weight: 600; border: 1px solid #273171;\">Release criterion<\/th>\n<th style=\"background: #273171; color: #ffffff; padding: 12px 14px; text-align: left; font-weight: 600; border: 1px solid #273171;\">Record<\/th>\n<\/tr>\n<\/thead>\n<tbody>\n<tr>\n<td style=\"border: 1px solid #E5E5E5; padding: 10px 14px;\">Chemistry<\/td>\n<td style=\"border: 1px solid #E5E5E5; padding: 10px 14px;\">Spark-AES chill-cast disc<\/td>\n<td style=\"border: 1px solid #E5E5E5; padding: 10px 14px;\">Every heat, before tap<\/td>\n<td style=\"border: 1px solid #E5E5E5; padding: 10px 14px;\">Inside alloy limits<\/td>\n<td style=\"border: 1px solid #E5E5E5; padding: 10px 14px;\">Heat sheet, 3\u20137 yr retention<\/td>\n<\/tr>\n<tr style=\"background: #F5F5F5;\">\n<td style=\"border: 1px solid #E5E5E5; padding: 10px 14px;\">Hydrogen \/ DI<\/td>\n<td style=\"border: 1px solid #E5E5E5; padding: 10px 14px;\">Reduced-pressure sample<\/td>\n<td style=\"border: 1px solid #E5E5E5; padding: 10px 14px;\">Every ladle or transfer crucible<\/td>\n<td style=\"border: 1px solid #E5E5E5; padding: 10px 14px;\">DI \u2264 agreed limit (often 2.0%)<\/td>\n<td style=\"border: 1px solid #E5E5E5; padding: 10px 14px;\">Sample photo + value + time<\/td>\n<\/tr>\n<tr>\n<td style=\"border: 1px solid #E5E5E5; padding: 10px 14px;\">Modification \/ inoculation<\/td>\n<td style=\"border: 1px solid #E5E5E5; padding: 10px 14px;\">Thermal analysis cooling curve<\/td>\n<td style=\"border: 1px solid #E5E5E5; padding: 10px 14px;\">Every ladle for critical parts<\/td>\n<td style=\"border: 1px solid #E5E5E5; padding: 10px 14px;\">\u0394TE 8\u201312 \u00b0C (Al) \/ chill \u2264 3 mm (Fe)<\/td>\n<td style=\"border: 1px solid #E5E5E5; padding: 10px 14px;\">Curve file tied to heat number<\/td>\n<\/tr>\n<tr style=\"background: #F5F5F5;\">\n<td style=\"border: 1px solid #E5E5E5; padding: 10px 14px;\">Cleanliness<\/td>\n<td style=\"border: 1px solid #E5E5E5; padding: 10px 14px;\">Fracture sample, filter inspection<\/td>\n<td style=\"border: 1px solid #E5E5E5; padding: 10px 14px;\">Each pour setup<\/td>\n<td style=\"border: 1px solid #E5E5E5; padding: 10px 14px;\">No continuous oxide film<\/td>\n<td style=\"border: 1px solid #E5E5E5; padding: 10px 14px;\">Photo + filter ppi \/ lot<\/td>\n<\/tr>\n<tr>\n<td style=\"border: 1px solid #E5E5E5; padding: 10px 14px;\">Temperature<\/td>\n<td style=\"border: 1px solid #E5E5E5; padding: 10px 14px;\">Immersion thermocouple<\/td>\n<td style=\"border: 1px solid #E5E5E5; padding: 10px 14px;\">Each ladle<\/td>\n<td style=\"border: 1px solid #E5E5E5; padding: 10px 14px;\">Within the agreed pouring window<\/td>\n<td style=\"border: 1px solid #E5E5E5; padding: 10px 14px;\">Value + timestamp<\/td>\n<\/tr>\n<tr style=\"background: #F5F5F5;\">\n<td style=\"border: 1px solid #E5E5E5; padding: 10px 14px;\">Final verification<\/td>\n<td style=\"border: 1px solid #E5E5E5; padding: 10px 14px;\">Radiography per <a style=\"color: #086ad4; text-decoration: none;\" href=\"https:\/\/store.astm.org\/standards\/e155\" target=\"_blank\" rel=\"noopener\">ASTM E155<\/a> where specified<\/td>\n<td style=\"border: 1px solid #E5E5E5; padding: 10px 14px;\">Per sampling plan<\/td>\n<td style=\"border: 1px solid #E5E5E5; padding: 10px 14px;\">Agreed severity level<\/td>\n<td style=\"border: 1px solid #E5E5E5; padding: 10px 14px;\">Report linked to heat number<\/td>\n<\/tr>\n<\/tbody>\n<\/table>\n<h3 style=\"font-family: 'Poppins',sans-serif; color: #273171; font-size: 20px; font-weight: 600; line-height: 1.4; margin: 26px 0 8px; text-transform: capitalize;\">Three gates, one heat number<\/h3>\n<hr style=\"width: 100px; height: 4px; background: #EF890D; border: none; border-radius: 2px; margin: 0 0 14px; line-height: 0; opacity: 1;\" \/>\n<p style=\"margin: 0 0 18px;\">In a mature casting melt treatment system, the release logic is binary: chemistry, DI and thermal analysis all pass before the ladle is released; one failure sends the metal back for re-treatment rather than into a mold. Every record carries the same heat number that appears on the casting batch, the <a style=\"color: #086ad4; text-decoration: none;\" href=\"https:\/\/chinametalfoundry.com\/pl\/blog\/casting-first-article-inspection\/\" target=\"_blank\" rel=\"noopener\">kontrola pierwszej partii<\/a> report and the certificate. That single linkage is what turns a pile of measurements into traceability \u2014 and it is what a buyer needs when a field failure happens 18 months later.<\/p>\n<p style=\"margin: 0 0 18px;\">Tie the same data into the <a style=\"color: #086ad4; text-decoration: none;\" href=\"https:\/\/chinametalfoundry.com\/pl\/blog\/przewodnik-po-tolerancjach-odlewniczych\/\" target=\"_blank\" rel=\"noopener\">tolerances guide<\/a> and the <a style=\"color: #086ad4; text-decoration: none;\" href=\"https:\/\/chinametalfoundry.com\/pl\/blog\/umowa-dotyczaca-jakosci-odlewow\/\" target=\"_blank\" rel=\"noopener\">quality agreement<\/a>: dimensional capability depends on consistent solidification behaviour, and inconsistent melt condition shows up as scatter in shrinkage allowance long before it shows up as outright scrap. If the supplier audits are upcoming, ask for the raw DI and \u0394TE logs, not a summary certificate.<\/p>\n<h2 style=\"font-family: 'Poppins',sans-serif; color: #273171; font-size: 25px; font-weight: 600; line-height: 1.3; margin: 34px 0 14px; padding: 4px 0 4px 30px; background: linear-gradient(to right, #ff512f 0px, #dd2476 5px, transparent 5px);\">What Casting Melt Treatment Costs and Where It Pays Back<\/h2>\n<p style=\"margin: 0 0 18px;\">Buyers often resist paying for melt control because it is invisible in the unit price. The arithmetic is straightforward once the yield effect is written down. Worked case: 60,000 A356 sand castings per year at 4.2 kg net each, fully loaded cost USD 18.40 per poured casting, baseline scrap 6.0%. Adding rotary degassing, filtration and ladle-by-ladle DI \/ thermal-analysis checks brings scrap to 3.6%.<\/p>\n<p style=\"margin: 0 0 18px;\">At 6.0% scrap, the foundry must pour 60,000 \/ 0.940 = <strong style=\"color: #273171;\">63,830<\/strong> castings to ship 60,000. At 3.6%, it pours 60,000 \/ 0.964 = <strong style=\"color: #273171;\">62,240<\/strong>. The difference is 1,590 castings that no longer consume metal, melting energy, molding time and cleaning labour: 1,590 \u00d7 USD 18.40 = <strong style=\"color: #273171;\">USD 29,256 per year<\/strong>. The treatment package costs USD 11,800 per year (rotor and gas, filters, master alloy, quick-cup consumables, sampling labour), leaving USD 17,456 net and a payback of about 8.1 months.<\/p>\n<table style=\"width: 100%; border-collapse: collapse; margin: 18px 0 24px; font-size: 15px; color: #333333;\">\n<thead>\n<tr>\n<th style=\"background: #273171; color: #ffffff; padding: 12px 14px; text-align: left; font-weight: 600; border: 1px solid #273171;\">Measure<\/th>\n<th style=\"background: #273171; color: #ffffff; padding: 12px 14px; text-align: left; font-weight: 600; border: 1px solid #273171;\">Annual cost (USD)<\/th>\n<th style=\"background: #273171; color: #ffffff; padding: 12px 14px; text-align: left; font-weight: 600; border: 1px solid #273171;\">Scrap rate<\/th>\n<th style=\"background: #273171; color: #ffffff; padding: 12px 14px; text-align: left; font-weight: 600; border: 1px solid #273171;\">Gross saving (USD\/yr)<\/th>\n<th style=\"background: #273171; color: #ffffff; padding: 12px 14px; text-align: left; font-weight: 600; border: 1px solid #273171;\">Net (USD\/yr)<\/th>\n<th style=\"background: #273171; color: #ffffff; padding: 12px 14px; text-align: left; font-weight: 600; border: 1px solid #273171;\">Payback<\/th>\n<\/tr>\n<\/thead>\n<tbody>\n<tr>\n<td style=\"border: 1px solid #E5E5E5; padding: 10px 14px;\">Baseline (no formal control)<\/td>\n<td style=\"border: 1px solid #E5E5E5; padding: 10px 14px;\">0<\/td>\n<td style=\"border: 1px solid #E5E5E5; padding: 10px 14px;\">6.0%<\/td>\n<td style=\"border: 1px solid #E5E5E5; padding: 10px 14px;\">\u2014<\/td>\n<td style=\"border: 1px solid #E5E5E5; padding: 10px 14px;\">\u2014<\/td>\n<td style=\"border: 1px solid #E5E5E5; padding: 10px 14px;\">\u2014<\/td>\n<\/tr>\n<tr style=\"background: #F5F5F5;\">\n<td style=\"border: 1px solid #E5E5E5; padding: 10px 14px;\">Rotary degassing + DI checks<\/td>\n<td style=\"border: 1px solid #E5E5E5; padding: 10px 14px;\">4,200<\/td>\n<td style=\"border: 1px solid #E5E5E5; padding: 10px 14px;\">4.6%<\/td>\n<td style=\"border: 1px solid #E5E5E5; padding: 10px 14px;\">16,560<\/td>\n<td style=\"border: 1px solid #E5E5E5; padding: 10px 14px;\">12,360<\/td>\n<td style=\"border: 1px solid #E5E5E5; padding: 10px 14px;\">4.1 months<\/td>\n<\/tr>\n<tr>\n<td style=\"border: 1px solid #E5E5E5; padding: 10px 14px;\">Add ceramic foam filtration<\/td>\n<td style=\"border: 1px solid #E5E5E5; padding: 10px 14px;\">3,100<\/td>\n<td style=\"border: 1px solid #E5E5E5; padding: 10px 14px;\">4.0%<\/td>\n<td style=\"border: 1px solid #E5E5E5; padding: 10px 14px;\">23,460<\/td>\n<td style=\"border: 1px solid #E5E5E5; padding: 10px 14px;\">16,160<\/td>\n<td style=\"border: 1px solid #E5E5E5; padding: 10px 14px;\">4.9 months<\/td>\n<\/tr>\n<tr style=\"background: #F5F5F5;\">\n<td style=\"border: 1px solid #E5E5E5; padding: 10px 14px;\">Add thermal analysis per ladle<\/td>\n<td style=\"border: 1px solid #E5E5E5; padding: 10px 14px;\">2,400<\/td>\n<td style=\"border: 1px solid #E5E5E5; padding: 10px 14px;\">3.7%<\/td>\n<td style=\"border: 1px solid #E5E5E5; padding: 10px 14px;\">27,600<\/td>\n<td style=\"border: 1px solid #E5E5E5; padding: 10px 14px;\">17,900<\/td>\n<td style=\"border: 1px solid #E5E5E5; padding: 10px 14px;\">6.3 months<\/td>\n<\/tr>\n<tr>\n<td style=\"border: 1px solid #E5E5E5; padding: 10px 14px;\">Full package above<\/td>\n<td style=\"border: 1px solid #E5E5E5; padding: 10px 14px;\">11,800<\/td>\n<td style=\"border: 1px solid #E5E5E5; padding: 10px 14px;\">3.6%<\/td>\n<td style=\"border: 1px solid #E5E5E5; padding: 10px 14px;\">29,256<\/td>\n<td style=\"border: 1px solid #E5E5E5; padding: 10px 14px;\">17,456<\/td>\n<td style=\"border: 1px solid #E5E5E5; padding: 10px 14px;\">8.1 months<\/td>\n<\/tr>\n<tr style=\"background: #F5F5F5;\">\n<td style=\"border: 1px solid #E5E5E5; padding: 10px 14px;\">Same package, gray iron counterweights<\/td>\n<td style=\"border: 1px solid #E5E5E5; padding: 10px 14px;\">9,600<\/td>\n<td style=\"border: 1px solid #E5E5E5; padding: 10px 14px;\">1.8% \u2192 1.3%<\/td>\n<td style=\"border: 1px solid #E5E5E5; padding: 10px 14px;\">3,100<\/td>\n<td style=\"border: 1px solid #E5E5E5; padding: 10px 14px;\">\u22126,500<\/td>\n<td style=\"border: 1px solid #E5E5E5; padding: 10px 14px;\">Never<\/td>\n<\/tr>\n<\/tbody>\n<\/table>\n<h3 style=\"font-family: 'Poppins',sans-serif; color: #273171; font-size: 20px; font-weight: 600; line-height: 1.4; margin: 26px 0 8px; text-transform: capitalize;\">Who keeps the yield gain<\/h3>\n<hr style=\"width: 100px; height: 4px; background: #EF890D; border: none; border-radius: 2px; margin: 0 0 14px; line-height: 0; opacity: 1;\" \/>\n<p style=\"margin: 0 0 18px;\">The last row is the useful counterexample: on a non-critical gray iron counterweight with no radiographic requirement, the same package loses money. Casting melt treatment should be specified where the consequence of failure is real \u2014 pressure tightness, fatigue loading, structural T6 properties \u2014 not applied as a blanket surcharge. The second question is contractual: if the foundry cuts scrap from 6% to 3.6%, does the unit price fall at the next review, or does the supplier keep the gain until the tooling is amortized? Write it into the <a style=\"color: #086ad4; text-decoration: none;\" href=\"https:\/\/chinametalfoundry.com\/pl\/blog\/casting-price-adjustment\/\" target=\"_blank\" rel=\"noopener\">price adjustment clause<\/a> or the <a style=\"color: #086ad4; text-decoration: none;\" href=\"https:\/\/chinametalfoundry.com\/pl\/blog\/umowa-dotyczaca-jakosci-odlewow\/\" target=\"_blank\" rel=\"noopener\">quality agreement<\/a>; otherwise a <a style=\"color: #086ad4; text-decoration: none;\" href=\"https:\/\/chinametalfoundry.com\/pl\/blog\/casting-rfq\/\" target=\"_blank\" rel=\"noopener\">repeat RFQ<\/a> quietly resets the baseline. Our <a style=\"color: #086ad4; text-decoration: none;\" href=\"https:\/\/chinametalfoundry.com\/pl\/blog\/podzial-kosztow-rzucania-zaklec\/\" target=\"_blank\" rel=\"noopener\">cost breakdown<\/a> oraz <a style=\"color: #086ad4; text-decoration: none;\" href=\"https:\/\/chinametalfoundry.com\/pl\/blog\/casting-price-per-kg\/\" target=\"_blank\" rel=\"noopener\">price-per-kg analysis<\/a> show where yield assumptions hide in a quote.<\/p>\n<p style=\"margin: 0 0 18px;\">Casting melt treatment pays twice: there is a scheduling benefit too. Fewer rejected castings means fewer remake queues, which shows up as delivery reliability rather than price; the <a style=\"color: #086ad4; text-decoration: none;\" href=\"https:\/\/chinametalfoundry.com\/pl\/blog\/casting-lead-time\/\" target=\"_blank\" rel=\"noopener\">lead-time model<\/a> treats yield as a capacity multiplier. Buyers who reserve <a style=\"color: #086ad4; text-decoration: none;\" href=\"https:\/\/chinametalfoundry.com\/pl\/metal-prototype-casting-services\/\" target=\"_blank\" rel=\"noopener\">prototype capacity<\/a> or use <a style=\"color: #086ad4; text-decoration: none;\" href=\"https:\/\/chinametalfoundry.com\/pl\/prototyp-wykonany-metoda-druku-3d\/\" target=\"_blank\" rel=\"noopener\">3D-printed patterns<\/a> for a bridge build should carry the same melt specification into production, or the prototype properties will not reproduce.<\/p>\n<h2 style=\"font-family: 'Poppins',sans-serif; color: #273171; font-size: 25px; font-weight: 600; line-height: 1.3; margin: 34px 0 14px; padding: 4px 0 4px 30px; background: linear-gradient(to right, #ff512f 0px, #dd2476 5px, transparent 5px);\">Specifying Casting Melt Treatment in the RFQ and PO<\/h2>\n<p style=\"margin: 0 0 18px;\">If it is not written into the enquiry, it will not be quoted, and if it is not quoted it will not be done. A usable casting melt treatment specification has eight fields. Each one needs a number or a named method \u2014 &#8220;good foundry practice&#8221; is not an acceptance criterion.<\/p>\n<table style=\"width: 100%; border-collapse: collapse; margin: 18px 0 24px; font-size: 15px; color: #333333;\">\n<thead>\n<tr>\n<th style=\"background: #273171; color: #ffffff; padding: 12px 14px; text-align: left; font-weight: 600; border: 1px solid #273171;\">Field<\/th>\n<th style=\"background: #273171; color: #ffffff; padding: 12px 14px; text-align: left; font-weight: 600; border: 1px solid #273171;\">What to write<\/th>\n<th style=\"background: #273171; color: #ffffff; padding: 12px 14px; text-align: left; font-weight: 600; border: 1px solid #273171;\">Evidence to request<\/th>\n<\/tr>\n<\/thead>\n<tbody>\n<tr>\n<td style=\"border: 1px solid #E5E5E5; padding: 10px 14px;\">Alloy and charge<\/td>\n<td style=\"border: 1px solid #E5E5E5; padding: 10px 14px;\">Alloy designation + max 30\u201340% returns, degreased and dried<\/td>\n<td style=\"border: 1px solid #E5E5E5; padding: 10px 14px;\">Heat sheet, charge log<\/td>\n<\/tr>\n<tr style=\"background: #F5F5F5;\">\n<td style=\"border: 1px solid #E5E5E5; padding: 10px 14px;\">Degassing<\/td>\n<td style=\"border: 1px solid #E5E5E5; padding: 10px 14px;\">Rotary Ar\/N\u2082 degassing; DI \u2264 2.0% per ladle; re-test after 10 min<\/td>\n<td style=\"border: 1px solid #E5E5E5; padding: 10px 14px;\">DI value, time, sample photo<\/td>\n<\/tr>\n<tr>\n<td style=\"border: 1px solid #E5E5E5; padding: 10px 14px;\">Modification \/ inoculation<\/td>\n<td style=\"border: 1px solid #E5E5E5; padding: 10px 14px;\">Sr 100\u2013200 ppm residual (Al) or residual Mg 0.03\u20130.06% + late inoculation (Fe)<\/td>\n<td style=\"border: 1px solid #E5E5E5; padding: 10px 14px;\">Thermal-analysis curve, chill wedge<\/td>\n<\/tr>\n<tr style=\"background: #F5F5F5;\">\n<td style=\"border: 1px solid #E5E5E5; padding: 10px 14px;\">Filtration<\/td>\n<td style=\"border: 1px solid #E5E5E5; padding: 10px 14px;\">20 ppi \u00d7 20 mm ceramic foam in runner, flow \u2264 1.0 kg\/s per 100 \u00d7 100 mm<\/td>\n<td style=\"border: 1px solid #E5E5E5; padding: 10px 14px;\">Filter lot + setup photo<\/td>\n<\/tr>\n<tr>\n<td style=\"border: 1px solid #E5E5E5; padding: 10px 14px;\">Chemistry<\/td>\n<td style=\"border: 1px solid #E5E5E5; padding: 10px 14px;\">Spark-AES per <a style=\"color: #086ad4; text-decoration: none;\" href=\"https:\/\/store.astm.org\/standards\/e1251\" target=\"_blank\" rel=\"noopener\">ASTM E1251<\/a>, before tap<\/td>\n<td style=\"border: 1px solid #E5E5E5; padding: 10px 14px;\">Signed heat certificate<\/td>\n<\/tr>\n<tr style=\"background: #F5F5F5;\">\n<td style=\"border: 1px solid #E5E5E5; padding: 10px 14px;\">Release gate<\/td>\n<td style=\"border: 1px solid #E5E5E5; padding: 10px 14px;\">All three gates pass; failed ladle re-treated, never poured<\/td>\n<td style=\"border: 1px solid #E5E5E5; padding: 10px 14px;\">Ladle release log<\/td>\n<\/tr>\n<tr>\n<td style=\"border: 1px solid #E5E5E5; padding: 10px 14px;\">Traceability<\/td>\n<td style=\"border: 1px solid #E5E5E5; padding: 10px 14px;\">Heat number on casting batch, FAI and certificate; records 3\u20137 yr<\/td>\n<td style=\"border: 1px solid #E5E5E5; padding: 10px 14px;\">Traceability matrix<\/td>\n<\/tr>\n<tr style=\"background: #F5F5F5;\">\n<td style=\"border: 1px solid #E5E5E5; padding: 10px 14px;\">Verification<\/td>\n<td style=\"border: 1px solid #E5E5E5; padding: 10px 14px;\">Radiographic class per <a style=\"color: #086ad4; text-decoration: none;\" href=\"https:\/\/store.astm.org\/standards\/e155\" target=\"_blank\" rel=\"noopener\">ASTM E155<\/a> where applicable<\/td>\n<td style=\"border: 1px solid #E5E5E5; padding: 10px 14px;\">Radiographic report<\/td>\n<\/tr>\n<\/tbody>\n<\/table>\n<ul style=\"margin: 0 0 18px; padding-left: 22px;\">\n<li style=\"margin: 0 0 8px;\"><strong style=\"color: #273171;\">Avoid vague standards.<\/strong> Writing &#8220;per applicable ASTM standards&#8221; without a DI limit or acceptance level leaves the supplier free to define the test. Name the method and the number.<\/li>\n<li style=\"margin: 0 0 8px;\"><strong style=\"color: #273171;\">Ask for raw logs.<\/strong> A summary certificate confirms that a test existed; raw DI and \u0394TE logs confirm when it was taken relative to the pour.<\/li>\n<li style=\"margin: 0 0 8px;\"><strong style=\"color: #273171;\">Link to disposition.<\/strong> Define upfront what happens when a heat is poured out of specification \u2014 see the <a style=\"color: #086ad4; text-decoration: none;\" href=\"https:\/\/chinametalfoundry.com\/pl\/blog\/casting-nonconformance\/\" target=\"_blank\" rel=\"noopener\">nonconformance framework<\/a> for the four disposition paths.<\/li>\n<\/ul>\n<p style=\"margin: 0 0 18px;\">Match casting melt treatment stringency to the route. <a style=\"color: #086ad4; text-decoration: none;\" href=\"https:\/\/chinametalfoundry.com\/pl\/odlewanie-w-formach-piaskowych\/\" target=\"_blank\" rel=\"noopener\">Odlewanie w formach piaskowych<\/a> of large structural housings justifies the full package; <a style=\"color: #086ad4; text-decoration: none;\" href=\"https:\/\/chinametalfoundry.com\/pl\/odlewanie-precyzyjne\/\" target=\"_blank\" rel=\"noopener\">odlewanie precyzyjne<\/a> of small precision parts adds tight filtration and temperature control; <a style=\"color: #086ad4; text-decoration: none;\" href=\"https:\/\/chinametalfoundry.com\/pl\/uslugi-odlewania-cisnieniowego\/\" target=\"_blank\" rel=\"noopener\">high-pressure die casting<\/a> needs inline degassing and a short hold time rather than ladle-by-ladle sampling. Tooling decisions <a style=\"color: #086ad4; text-decoration: none;\" href=\"https:\/\/chinametalfoundry.com\/pl\/casting-molds-making\/\" target=\"_blank\" rel=\"noopener\">wytwarzanie form<\/a> oraz <a style=\"color: #086ad4; text-decoration: none;\" href=\"https:\/\/chinametalfoundry.com\/pl\/blog\/casting-tooling-cost\/\" target=\"_blank\" rel=\"noopener\">tooling cost<\/a> are separate from melt control, but both belong in the same <a style=\"color: #086ad4; text-decoration: none;\" href=\"https:\/\/chinametalfoundry.com\/pl\/blog\/casting-rfq\/\" target=\"_blank\" rel=\"noopener\">RFQ data pack<\/a> so the quoted yield assumption is visible.<\/p>\n<h2 style=\"font-family: 'Poppins',sans-serif; color: #273171; font-size: 25px; font-weight: 600; line-height: 1.3; margin: 34px 0 14px; padding: 4px 0 4px 30px; background: linear-gradient(to right, #ff512f 0px, #dd2476 5px, transparent 5px);\">Najcz\u0119\u015bciej zadawane pytania<\/h2>\n<h3 style=\"font-family: 'Poppins',sans-serif; color: #273171; font-size: 20px; font-weight: 600; line-height: 1.4; margin: 26px 0 8px; text-transform: capitalize;\">Is casting melt treatment the same as heat treatment?<\/h3>\n<p style=\"margin: 0 0 18px;\">No. Melt treatment happens to liquid metal before pouring and controls gas, inclusions and nucleation. Heat treatment happens to the solid casting afterwards and controls precipitates, matrix phases and stress relief. T6 cannot remove hydrogen porosity; degassing cannot produce a T6 temper. Both are needed for structural aluminum parts.<\/p>\n<h3 style=\"font-family: 'Poppins',sans-serif; color: #273171; font-size: 20px; font-weight: 600; line-height: 1.4; margin: 26px 0 8px; text-transform: capitalize;\">Can vacuum impregnation fix hydrogen porosity?<\/h3>\n<p style=\"margin: 0 0 18px;\">It can seal connected pores enough to pass a leak test, but it does not restore fatigue strength or fix a coarse, unmodified microstructure. <a style=\"color: #086ad4; text-decoration: none;\" href=\"https:\/\/chinametalfoundry.com\/pl\/blog\/aluminum-castings-vacuum-impregnation\/\" target=\"_blank\" rel=\"noopener\">Vacuum impregnation<\/a> is a salvage route, not a substitute for melt control, and most quality agreements exclude it as a default disposition.<\/p>\n<h3 style=\"font-family: 'Poppins',sans-serif; color: #273171; font-size: 20px; font-weight: 600; line-height: 1.4; margin: 26px 0 8px; text-transform: capitalize;\">What density index should I specify for a structural A356 casting?<\/h3>\n<p style=\"margin: 0 0 18px;\">DI \u2264 2.0% is a practical production limit for structural parts, with \u2264 1.0% for pressure-tight or radiographically critical housings. Set the limit together with the radiographic class; a very tight DI on a non-critical part buys nothing and raises the quote.<\/p>\n<h3 style=\"font-family: 'Poppins',sans-serif; color: #273171; font-size: 20px; font-weight: 600; line-height: 1.4; margin: 26px 0 8px; text-transform: capitalize;\">Does melt treatment change the quoted price per kg?<\/h3>\n<p style=\"margin: 0 0 18px;\">Usually by a small line item \u2014 consumables, sampling labour and yield allowance. The larger effect is on how many castings must be poured to ship the ordered quantity, which is why the <a style=\"color: #086ad4; text-decoration: none;\" href=\"https:\/\/chinametalfoundry.com\/pl\/blog\/casting-price-per-kg\/\" target=\"_blank\" rel=\"noopener\">price-per-kg comparison<\/a> and the yield assumption should be quoted together.<\/p>\n<h3 style=\"font-family: 'Poppins',sans-serif; color: #273171; font-size: 20px; font-weight: 600; line-height: 1.4; margin: 26px 0 8px; text-transform: capitalize;\">How often should a foundry record melt treatment data?<\/h3>\n<p style=\"margin: 0 0 18px;\">Chemistry per heat; DI and thermal analysis per ladle for critical parts; filter and temperature checks per pour setup. Records should carry the heat number and be retained 3\u20137 years, matching the <a style=\"color: #086ad4; text-decoration: none;\" href=\"https:\/\/chinametalfoundry.com\/pl\/blog\/casting-first-article-inspection\/\" target=\"_blank\" rel=\"noopener\">FAI<\/a> and certificate retention.<\/p>\n<h3 style=\"font-family: 'Poppins',sans-serif; color: #273171; font-size: 20px; font-weight: 600; line-height: 1.4; margin: 26px 0 8px; text-transform: capitalize;\">Can I skip casting melt treatment for prototype castings?<\/h3>\n<p style=\"margin: 0 0 18px;\">Only if the prototype is purely for fit and form. If mechanical test data from the prototype will be used to approve production, skip it and you will qualify a different material. Keep the same specification through <a style=\"color: #086ad4; text-decoration: none;\" href=\"https:\/\/chinametalfoundry.com\/pl\/metal-prototype-casting-services\/\" target=\"_blank\" rel=\"noopener\">odlewanie prototypowe<\/a> and production, or re-qualify explicitly.<\/p>\n\t\t<div data-elementor-type=\"section\" data-elementor-id=\"3550\" class=\"elementor elementor-3550\" data-elementor-post-type=\"elementor_library\">\n\t\t\t\t\t<section class=\"elementor-section elementor-top-section elementor-element elementor-element-19b1acf1 elementor-section-boxed elementor-section-height-default elementor-section-height-default\" data-id=\"19b1acf1\" data-element_type=\"section\" data-e-type=\"section\" data-settings=\"{&quot;background_background&quot;:&quot;classic&quot;,&quot;ekit_has_onepagescroll_dot&quot;:&quot;yes&quot;}\">\n\t\t\t\t\t\t\t<div class=\"elementor-background-overlay\"><\/div>\n\t\t\t\t\t\t\t<div class=\"elementor-container elementor-column-gap-default\">\n\t\t\t\t\t<div class=\"elementor-column elementor-col-100 elementor-top-column elementor-element elementor-element-56e26ed6\" data-id=\"56e26ed6\" data-element_type=\"column\" data-e-type=\"column\">\n\t\t\t<div class=\"elementor-widget-wrap elementor-element-populated\">\n\t\t\t\t\t\t<div class=\"elementor-element elementor-element-52c3d00c elementor-widget elementor-widget-elementskit-heading\" data-id=\"52c3d00c\" data-element_type=\"widget\" data-e-type=\"widget\" data-settings=\"{&quot;ekit_we_effect_on&quot;:&quot;none&quot;}\" data-widget_type=\"elementskit-heading.default\">\n\t\t\t\t<div class=\"elementor-widget-container\">\n\t\t\t\t\t<div class=\"ekit-wid-con\" ><div class=\"ekit-heading elementskit-section-title-wraper text_left   ekit_heading_tablet-   ekit_heading_mobile-\"><h3 class=\"ekit-heading--title elementskit-section-title\">Szukasz niezawodnej odlewni metali w Chinach?<\/h3><\/div><\/div>\t\t\t\t<\/div>\n\t\t\t\t<\/div>\n\t\t\t\t<div class=\"elementor-element elementor-element-24c75aa0 elementor-widget elementor-widget-text-editor\" data-id=\"24c75aa0\" data-element_type=\"widget\" data-e-type=\"widget\" data-settings=\"{&quot;ekit_we_effect_on&quot;:&quot;none&quot;}\" data-widget_type=\"text-editor.default\">\n\t\t\t\t<div class=\"elementor-widget-container\">\n\t\t\t\t\t\t\t\t\t<ul><li>Mo\u017cemy pom\u00f3c Ci zoptymalizowa\u0107 projekt produktu i obni\u017cy\u0107 koszty.<\/li><li>Mo\u017cemy pom\u00f3c Pa\u0144stwu w zakresie wysokiej jako\u015bci odlew\u00f3w produkowanych w du\u017cych ilo\u015bciach.<\/li><li>Mo\u017cemy dostarczy\u0107 na czas i zyska\u0107 wi\u0119cej mo\u017cliwo\u015bci rynkowych sprzeda\u017cy.<\/li><li>Skorzystaj z us\u0142ug odlewniczych firmy Supro MFG.<\/li><\/ul>\t\t\t\t\t\t\t\t<\/div>\n\t\t\t\t<\/div>\n\t\t\t\t<div class=\"elementor-element elementor-element-51a20937 elementor-align-left elementor-widget elementor-widget-global elementor-global-1143 elementor-widget-button\" data-id=\"51a20937\" data-element_type=\"widget\" data-e-type=\"widget\" data-settings=\"{&quot;ekit_we_effect_on&quot;:&quot;none&quot;}\" data-widget_type=\"button.default\">\n\t\t\t\t<div class=\"elementor-widget-container\">\n\t\t\t\t\t\t\t\t\t<div class=\"elementor-button-wrapper\">\n\t\t\t\t\t<a class=\"elementor-button elementor-button-link elementor-size-sm elementor-animation-grow\" href=\"https:\/\/chinametalfoundry.com\/pl\/kontakt\/\">\n\t\t\t\t\t\t<span class=\"elementor-button-content-wrapper\">\n\t\t\t\t\t\t\t\t\t<span class=\"elementor-button-text\">Popro\u015b o wycen\u0119 bezpo\u015brednio od producenta <\/span>\n\t\t\t\t\t<\/span>\n\t\t\t\t\t<\/a>\n\t\t\t\t<\/div>\n\t\t\t\t\t\t\t\t<\/div>\n\t\t\t\t<\/div>\n\t\t\t\t\t<\/div>\n\t\t<\/div>\n\t\t\t\t\t<\/div>\n\t\t<\/section>\n\t\t\t\t<\/div>\n\t\t\n<p class=\"sc-note\" style=\"font-size: 13px; color: #9a9a9a; margin: 28px 0 0;\">*Data referenced from ASTM E1251 \/ E155, Aluminum Association publications and Supro MFG shop-floor records. Values are typical production ranges; confirm limits for your alloy, section thickness and acceptance class with your foundry.<\/p>\n<\/article>","protected":false},"excerpt":{"rendered":"<p>Casting melt treatment is the short sequence of steps applied to metal between the furnace and the mold, and it [&hellip;]<\/p>\n","protected":false},"author":5,"featured_media":8431,"comment_status":"closed","ping_status":"closed","sticky":false,"template":"","format":"standard","meta":{"site-sidebar-layout":"default","site-content-layout":"","ast-site-content-layout":"default","site-content-style":"default","site-sidebar-style":"default","ast-global-header-display":"","ast-banner-title-visibility":"","ast-main-header-display":"","ast-hfb-above-header-display":"","ast-hfb-below-header-display":"","ast-hfb-mobile-header-display":"","site-post-title":"","ast-breadcrumbs-content":"","ast-featured-img":"","footer-sml-layout":"","ast-disable-related-posts":"","theme-transparent-header-meta":"default","adv-header-id-meta":"","stick-header-meta":"default","header-above-stick-meta":"","header-main-stick-meta":"","header-below-stick-meta":"","astra-migrate-meta-layouts":"set","ast-page-background-enabled":"default","ast-page-background-meta":{"desktop":{"background-color":"var(--ast-global-color-4)","background-image":"","background-repeat":"repeat","background-position":"center center","background-size":"auto","background-attachment":"scroll","background-type":"","background-media":"","overlay-type":"","overlay-color":"","overlay-opacity":"","overlay-gradient":""},"tablet":{"background-color":"","background-image":"","background-repeat":"repeat","background-position":"center center","background-size":"auto","background-attachment":"scroll","background-type":"","background-media":"","overlay-type":"","overlay-color":"","overlay-opacity":"","overlay-gradient":""},"mobile":{"background-color":"","background-image":"","background-repeat":"repeat","background-position":"center center","background-size":"auto","background-attachment":"scroll","background-type":"","background-media":"","overlay-type":"","overlay-color":"","overlay-opacity":"","overlay-gradient":""}},"ast-content-background-meta":{"desktop":{"background-color":"var(--ast-global-color-5)","background-image":"","background-repeat":"repeat","background-position":"center center","background-size":"auto","background-attachment":"scroll","background-type":"","background-media":"","overlay-type":"","overlay-color":"","overlay-opacity":"","overlay-gradient":""},"tablet":{"background-color":"var(--ast-global-color-5)","background-image":"","background-repeat":"repeat","background-position":"center center","background-size":"auto","background-attachment":"scroll","background-type":"","background-media":"","overlay-type":"","overlay-color":"","overlay-opacity":"","overlay-gradient":""},"mobile":{"background-color":"var(--ast-global-color-5)","background-image":"","background-repeat":"repeat","background-position":"center center","background-size":"auto","background-attachment":"scroll","background-type":"","background-media":"","overlay-type":"","overlay-color":"","overlay-opacity":"","overlay-gradient":""}},"footnotes":""},"categories":[51],"tags":[46,47,49,42],"class_list":["post-8430","post","type-post","status-publish","format-standard","has-post-thumbnail","hentry","category-casting-processes","tag-casting-materials","tag-casting-process","tag-manufacturing-process","tag-metal-casting"],"_links":{"self":[{"href":"https:\/\/chinametalfoundry.com\/pl\/wp-json\/wp\/v2\/posts\/8430","targetHints":{"allow":["GET"]}}],"collection":[{"href":"https:\/\/chinametalfoundry.com\/pl\/wp-json\/wp\/v2\/posts"}],"about":[{"href":"https:\/\/chinametalfoundry.com\/pl\/wp-json\/wp\/v2\/types\/post"}],"author":[{"embeddable":true,"href":"https:\/\/chinametalfoundry.com\/pl\/wp-json\/wp\/v2\/users\/5"}],"replies":[{"embeddable":true,"href":"https:\/\/chinametalfoundry.com\/pl\/wp-json\/wp\/v2\/comments?post=8430"}],"version-history":[{"count":5,"href":"https:\/\/chinametalfoundry.com\/pl\/wp-json\/wp\/v2\/posts\/8430\/revisions"}],"predecessor-version":[{"id":8592,"href":"https:\/\/chinametalfoundry.com\/pl\/wp-json\/wp\/v2\/posts\/8430\/revisions\/8592"}],"wp:featuredmedia":[{"embeddable":true,"href":"https:\/\/chinametalfoundry.com\/pl\/wp-json\/wp\/v2\/media\/8431"}],"wp:attachment":[{"href":"https:\/\/chinametalfoundry.com\/pl\/wp-json\/wp\/v2\/media?parent=8430"}],"wp:term":[{"taxonomy":"category","embeddable":true,"href":"https:\/\/chinametalfoundry.com\/pl\/wp-json\/wp\/v2\/categories?post=8430"},{"taxonomy":"post_tag","embeddable":true,"href":"https:\/\/chinametalfoundry.com\/pl\/wp-json\/wp\/v2\/tags?post=8430"}],"curies":[{"name":"wp","href":"https:\/\/api.w.org\/{rel}","templated":true}]}}